NIGRIN PERFORMANCE

Metal Filler 500 g 2 pcs

Item no. 72116

  • Permanently remains elastic & vibration-resistant

  • Reliably fills dents & precisely levels out deformations

  • Easy to sand, with reduced dust generation

Siegel

The pro­duct in de­tail


The NIGRIN PERFORMANCE Metal Filler is a high-quality, styrene-reduced two-component filler with aluminum powder — specially developed for repairing deformations on metal parts subject to high vibration stress. It is ideal for automotive body work and all applications where a permanently elastic and particularly durable fill is required.

After curing, the filler remains highly elastic, reliably levels out dents, and — thanks to its metal content — is exceptionally easy to sand, with significantly reduced dust generation. Its outstanding adhesion and filling capacity make it the PROFESSIONAL solution for demanding repair work.

Product benefits:

  • 490 g incl. 10 g hardener – styrene-reduced and user-friendly
  • Contains aluminum powder – for elasticity and vibration resistance
  • Ideal for heavily stressed metal parts and body panels
  • Reliably fills dents, cures crack-free and stably
  • Excellent sandability with minimal dust generation


Application steps

01

Ober­flä­che vor­be­rei­ten

Rost entfernen, entfetten, reinigen und die Oberfläche abschleifen.

02

Spach­tel an­mi­schen

PERFORMANCE Metal Filler mit Härter im Verhältnis 98% zu 2% mischen. Eine golfballgroße Menge Spachtel mit einer erbsengroßen Menge Härter gründlich vermischen.

03

Spach­tel auf­tra­gen

Die Mischung zügig verarbeiten, da die Aushärtung nach 3–4 Minuten beginnt.

04

Aus­här­ten las­sen

Ca. 20 Minuten aushärten lassen und die Oberfläche anschließend abschleifen.

05

Fi­nish durch­füh­ren

Die Reparaturstelle mit NIGRIN Feinfüller glätten und abschließend schleifen.

Note

Optimale Verarbeitungstemperatur über +10 °C. Weitere Informationen unter Karosserie-Reparaturschritte-Diagramm.